| Crystalline silicon in thin layerMuch less consumption of silicon. Only 2 µ k instead of some 100 µm is the crystalline layer of this new thin layer module of Sharp thick.Besides, nowadays 8.5% of efficiency are reached in the series and 10% in the research lab. |